Titanium (Ti) | Aluminum (Al) | Vanadium (V) | Tin (Sn) | |
Ti-6Al-4V | Rest | 5.5%-6.8% | 3.5%-4.5% | |
Ti-5Al-2.5Sn | Rest | 4.5%-5.5% | 2.0%-3.0% |
Density | 4.4-4.5g/cm³ |
Melting Point | 1660°C |
Coefficient of Thermal Expansion | 8-10×10⁻⁶/K (20°C-500°C) |
Thermal Conductivity | 6-22 W/(m·K) (depending on alloy grade) |
Electrical Resistivity | 0.14-0.17 μΩ·m |
Tensile Strength | 600-1200 MPa (depending on alloy grade) |
Yield Strength | 480-1100 MPa |
Elongation at Break | 10%-25% |
Hardness | 200-400 HB |
Steps | DZX Do | Time |
Confirmation of product parameters and application | We confirm the product according to the demand | Immediate |
Sample customization | In stock or confirm OEM/ODM customization | Immediate |
Production and processing | Confirmation of production as well as product testing | 7-15 days |
Packaging and Transportation | Using carton + preservative film + pallet | According to the national |
dlx-group@dlx-alloy.com | |
Phone | 0086-1990 6119 641 |
Address | NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu,China |