Grades | NC003 | NC005 | NC010 | NC012 | NC015 | NC020 | NC025 | NC030 | NC035 | NC040 | NC050 | |
CuNi1 | CuNi2 | CuNi6 | CuNi8 | CuNi10 | CuNi14 | CuNi19 | CuNi23 | CuNi30 | CuNi34 | CuNi44 | ||
Main Chemical Composition (%) | Nickel (Ni) | 1 | 2 | 6 | 8 | 10 | 14.2 | 19 | 23 | 30 | 34 | 44 |
Manganese (Mn) | / | / | / | / | / | 0.3 | 0.5 | 0.5 | 1 | 1 | 1 | |
Copper (Cu) | Rest | Rest | Rest | Rest | Rest | Rest | Rest | Rest | Rest | Rest | Rest |
Grades | NC003 | NC005 | NC010 | NC012 | NC015 | NC020 | NC025 | NC030 | NC035 | NC040 | NC050 |
CuNi1 | CuNi2 | CuNi6 | CuNi8 | CuNi10 | CuNi14 | CuNi19 | CuNi23 | CuNi30 | CuNi34 | CuNI44 | |
Max. Service Temperature (°C) | 200 | 200 | 220 | 250 | 250 | 300 | 300 | 300 | 350 | 350 | 400 |
Density (g/cm³) | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 |
Resistivity at 20℃ (μΩ·m) | 0.03±10% | 0.05±10% | 0.10±10% | 0.12±10% | 0.15±10% | 0.20±5% | 0.25±5% | 0.30±5% | 0.35±5% | 0.40±5% | 0.5±5% |
Resistance Temperature Coefficient ×10⁻⁶/ºC (20~600ºC) | <100 | <120 | <60 | <57 | <50 | <38 | <25 | <16 | <10 | 0 | 210 |
Tensile Strength (Mpa) | >210 | >220 | >250 | >270 | >290 | >310 | >340 | >350 | >400 | >400 | >420 |
Elongation at Rupture (%) | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 |
Melting Point (°C) | 1085 | 1090 | 1095 | 1097 | 1100 | 1115 | 1135 | 1150 | 1170 | 1180 | 1280 |
Thermoelectric Potential of Copper (μV/℃) (0~100℃) | -8 | -12 | -18 | -22 | -25 | -28 | -32 | -34 | -37 | -39 | -43 |
ISO | 13380, 197-6 |
ASTM | B111, B151, B466, B122 |
DIN | 86019, 17664 |
AMS | 12449, 12451 |
GB/T | 5231, 8890, 2059 |
Steps | DZX Do | Time |
Confirmation of product parameters and application | We confirm the product according to the demand | Immediate |
Sample customization | In stock or confirm OEM/ODM customization | Immediate |
Production and processing | Confirmation of production as well as product testing | 7-15 days |
Packaging and Transportation | Using carton + preservative film + pallet | According to the national |
Verify through material certifications and test reports provided by the supplier, ensuring compliance with industry standards.
Available as CuNi wire, tube, rod, plate, and more, customizable to specifications.
Typically requires cleaning to remove oxides; polishing or protective coatings may be applied based on use.
Select based on application needs, such as corrosion resistance or conductivity, and nickel content.
Relatively easy to process, supports drawing, forging, and welding, suitable for various manufacturing processes.
Marine engineering, shipbuilding, heat exchangers, power generation, and chemical equipment manufacturing.
Excellent corrosion resistance, good electrical and thermal conductivity, with high strength and ductility.
dlx-group@dlx-alloy.com | |
Phone | 0086-1990 6119 641 |
Address | NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu,China |