| Grades | Cr10Ni90 | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
| Main Chemical Composition (%) | Nickel (Ni) | 90 | Rest | Rest | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
| Chromium (Cr) | 10 | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
| Iron (Fe) | -- | ≤1.0 | ≤1.0 | Rest | Rest | Rest | |
| Grades | Cr10Ni90 | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 |
| Max. Service Temperature (°C) | 1300 | 1200 | 1250 | 1150 | 1100 | 1100 |
| Melting Point (°C) | 1400 | 1400 | 1380 | 1390 | 1390 | 1390 |
| Density (g/cm³) | 8.7 | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 |
| Resistivity at 20℃ (μΩ·m) | -- | 1.09±0.05 | 1.18±0.05 | 1.12±0.05 | 1.00±0.05 | 1.04±0.05 |
| Elongation at Rupture (%) | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 |
| Specific Heat (J/g.℃) | -- | 0.44 | 0.461 | 0.494 | 0.5 | 0.5 |
| Thermal Conductivity (KJ/m.h.ºC) | -- | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 |
| Coefficient of Lines Expansion (α×10⁻⁶/20~1000ºC) | -- | 18 | 17 | 17 | 19 | 19 |
| Micrographic Structure | -- | Austenite | Austenite | Austenite | Austenite | Austenite |
| Magnetic Properties | -- | Non-magnetic | Non-magnetic | Non-magnetic | Weak magnetic | Weak magnetic |
| ISO | 6208, 15156 |
| ASTM | B163, B166, B167, B168, B446 |
| DIN | 17742, 17750 |
| AMS | 5540, 5666 |
| GB/T | 1234, 2077, 4437 |
| Steps | DZX Do | Time |
| Confirmation of product parameters and application | We confirm the product according to the demand | Immediate |
| Sample customization | In stock or confirm OEM/ODM customization | Immediate |
| Production and processing | Confirmation of production as well as product testing | 7-15 days |
| Packaging and Transportation | Using carton + preservative film + pallet | According to the national |
| dlx-group@dlx-alloy.com | |
| Phone | 0086-1990 6119 641 |
| Address | NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu,China |